About this Abstract |
| Meeting |
2027 TMS Annual Meeting & Exhibition
|
| Symposium
|
Fatigue in Materials: Fundamentals, Multiscale Characterizations and Computational Modeling
|
| Presentation Title |
Fatigue and Fracture Behavior of Binder Jetted 17-4 PH Stainless Steel under Various Post-Processing Conditions |
| Author(s) |
Mohammadjavad Abdollahzadeh, Rudra NMI Patel, Meisam NMI Khademitab, Amir Mostafaei |
| On-Site Speaker (Planned) |
Mohammadjavad Abdollahzadeh |
| Abstract Scope |
This study examines the effects of powder reuse, sintering temperature (AS, 1360 vs. 1400°C), hot isostatic pressing (HIP), mechanical grinding (MG), and aging (AG) on the fatigue behavior of binder jetted 17-4 PH stainless steel under fully reversed axial loading (Rσ=-1). Higher sintering temperature improved fatigue performance, with 1400°C producing higher Basquin parameters, σf′=2304 MPa and b=–0.123, compared with 1360°C, σf′ = 1724 MPa and b = –0.113. Mechanical grinding was the dominant post-processing factor, reducing surface-defect-driven failures and improving high-cycle fatigue resistance, as shown by the shallower slope for 1400 AS+MG, b =-0.063. HIP further improved performance by closing internal pores, with HIP+MG conditions showing b=–0.064 to –0.079 and σf′=1373–1476 MPa. Aging provided limited improvement. Recycled powder negated the benefits of grinding, likely due to increased pores and open voids. Fractography confirmed surface-initiated cracking, while optimized HIP+MG produced fatigue performance competitive with laser powder bed fusion. |
| Proceedings Inclusion? |
Planned: |
| Keywords |
Additive Manufacturing, Iron and Steel, Characterization |