About this Abstract | 
  
   
    | Meeting | 
    MS&T21: Materials Science & Technology
       | 
  
   
    | Symposium 
       | 
    Powder Metallurgical Components in High Performance Applications
       | 
  
   
    | Presentation Title | 
    Development of Eco-friendly POM Binder System for High Strength Ti-MIM      | 
  
   
    | Author(s) | 
    Keemi  Lim, Muhammad  Dilawer  Hayat, Peng  Cao | 
  
   
    | On-Site Speaker (Planned) | 
    Keemi  Lim | 
  
   
    | Abstract Scope | 
    
The particular challenges related to the use of titanium and its alloy processed by MIM are its high reactivity and sensitivity towards contamination. In a typical MIM process, selections of appropriate binder and later removal have demonstrated to be crucial in reducing the contamination problem. The aim of this paper focuses on the development of a catalytic binder system based on polyacetal for Ti-MIM. An inherent characteristic of this catalytic binder system is their low debinding temperature at approximately 120-150 °C, which is below the temperature where impurities uptakes initiate (~ 260 °C). In addition, the effectiveness of employing organic acid as a potential green catalyst for the removal of polyacetal binder is reported.   |