| Abstract Scope |
Baffle former bolts are critical components in pressurized water reactor internals subjected to prolonged neutron irradiation. This work investigated the post-irradiation annealing response of two service-exposed bolts harvested from a commercial PWR after ~40 years of operation, spanning 15-41 dpa across head, mid-shank, and mid-thread regions. Isochronal anneals at 400, 550, 700, 850, and 1000°C for 1 hour, alongside an as-irradiated baseline, were applied to systematically recover dislocation loops, solute clusters, radiation-induced segregation, and cavities/bubbles. Micro indentation tracked region and dose dependent hardness recovery, while TEM/STEM quantified defect size, density, and coarsening behavior. FIB-milled micro-tensile specimens, tested in situ with EBSD, linked defect morphology to dislocation channel width, spacing, and strain localization. This study introduced a defect-morphology based framework testing whether cavity coarsening promoted cross-slip and reduced localization beyond dose-driven recovery alone, establishing a mechanistic basis for life-extension and inspection strategies for non-replaceable PWR reactor internals. |