Origin of hydrogen-related quasi-cleavage fracture in low-carbon steel |
| Author(s) |
Akinobu Shibata, Akiko Nakamura, Taku Moronaga, Kazuho Okada, Toru Hara |
| On-Site Speaker (Planned) |
Akinobu Shibata |
| Abstract Scope |
Hydrogen embrittlement becomes more severe with increasing material strength; therefore, improving hydrogen embrittlement resistance is essential for the practical use of advanced high-strength steels. Although the mechanism of hydrogen-related intergranular fracture is relatively straightforward, i.e., hydrogen-induced reduction of grain boundary cohesive energy, that of quasi-cleavage fracture remains insufficiently clarified. This study investigated hydrogen-related quasi-cleavage fracture behavior in low-carbon steel using three-dimensional crack characterization and detailed substructure observations. We found that local crack arrest occurred in regions where the resolved normal stress on the {011} planes was low. Isolated voids coalesced selectively on specific planes ahead of the main crack. Furthermore, void formation at dislocation cell boundaries and around tangled dislocation regions was observed. We propose that vacancies generated through dislocation interactions are stabilized by hydrogen, thereby promoting void formation through vacancy aggregation. The subsequent coalescence of these voids on {011} planes is a key process governing quasi-cleavage fracture. |
| Proceedings Inclusion? |
Planned: |
| Keywords |
Iron and Steel, Mechanical Properties, Characterization |