About this Abstract |
| Meeting |
2027 TMS Annual Meeting & Exhibition
|
| Symposium
|
Steels in Extreme Conditions III
|
| Presentation Title |
Hydrogen-related Fracture Behavior of Pre-strained Martensitic Steels with Different Carbide Morphology
|
| Author(s) |
Eri Nakagawa, Kazuho Okada, Taku Moronaga, Taisuke Sasaki, Akinobu Shibata |
| On-Site Speaker (Planned) |
Eri Nakagawa |
| Abstract Scope |
One of the most serious issues in the practical application of high-strength steels is hydrogen embrittlement (HE), a phenomenon in which the presence of hydrogen causes steels to become extremely brittle. Although plastic forming processes such as rolling are essential for the commercialization of steels, their effect on HE remains poorly understood. In this study, the effect of pre-strain on hydrogen-related fracture behavior was systematically investigated for tempered martensitic steels with ε-carbide and cementite. An Fe-3Mn-2Si-0.2C (wt.%) as-quenched martensitic steel was tempered at 300 to 500 ℃ for 400 to 1000 min, followed by cold rolling (reduction: 0 to 30%). As-heat-treated steels containing ε-carbides exhibited superior resistance to HE compared to those containing cementite. In contrast, while cold rolling reduced HE resistance in the tempered martensitic steel containing ε-carbides, it improved HE resistance in the cementite-precipitated steel. |
| Proceedings Inclusion? |
Planned: |
| Keywords |
Iron and Steel, Mechanical Properties, Characterization |