Efficient and selective extraction of tungsten from microwave-roasted scrap tungsten-cobalt (WC-Co) cemented carbide was systematically investigated via alkaline leaching. It was demonstrated that elevating the leaching temperature significantly promoted the dissolution of tungsten-bearing phases. Under the optimal conditions of a 2 mol/L NaOH solution, a liquid-to-solid ratio of 10 mL/g, a stirring rate of 500 rpm, and a leaching temperature of 130 ℃ for 90 min, a high tungsten leaching efficiency of 99.26% was achieved, accompanied by a residual tungsten content of only 4.57 wt.%. The microwave roasting process produced a loose, porous, and highly pulverized calcine (average particle size of 8.60 μm), which drastically shortened diffusion pathways and facilitated subsequent alkaline leaching. This study provides an environmentally friendly and highly efficient approach for high-value recycling of valuable metals from spent cemented carbides. |
| Proceedings Inclusion? |
Planned: |