| Abstract Scope |
Selenium-rich residues from copper refining are underutilized domestic sources of silver, gold, palladium, and platinum, but high selenium, tellurium, and bismuth contents hinder selective recovery. This study presents an integrated flowsheet for a residue containing 93.3 wt.% selenium, 1.23 wt.% tellurium, 0.282 wt.% bismuth, 0.0621 wt.% silver, 0.0600 wt.% palladium, 0.00640 wt.% platinum, and 0.0357 wt.% gold. Vacuum distillation at 400 oC volatilized selenium and tellurium, thereby enriching the target metals by more than 12-fold in the vacuum distillation residue (VDR). Water leaching of the VDR removed sodium sulfate, followed by hydrogen peroxide-hydrochloric acid leaching to dissolve gold, palladium, and platinum, while deporting silver as a silver chloride residue. Bismuth, selenium, and tellurium were rejected as a mixed byproduct by precipitation, and sequential solvent extraction recovered gold, palladium, and platinum. The integrated process recovered ≥80% of each target metal, establishing a route to convert selenium waste into precious metals. |