| Abstract Scope |
In this work, a two-stage recycling strategy based on a single HCOOH–H2O2 system was developed for the sequential recovery of lithium and other critical metals from mixed lithium-ion battery waste. In the first stage, selective lithium extraction was achieved, resulting in lithium recoveries exceeding 99% while the dissolution of Fe, Al, Ni, Co, Mn, and Cu remained below 1%. The resulting lithium-depleted residue was dominated by FePO4 and graphite but still contained valuable critical metals originating from mixed cathode materials and current collectors. In the second stage, the same reagent system was directly applied to the lithium-depleted residue without changing the leaching medium. Instead, selective recovery of critical metals was achieved through adjustment of reagent dosage and control of solution acidity and redox conditions. Under the optimum conditions, leaching efficiencies of 100% Ni, 99.1% Co, 91.8% Cu, and 71.2% Al were achieved, while Fe dissolution remained near 5%. |