| Abstract Scope |
Fe–Ni–C steels are promising for cryogenic structural applications because Ni lowers the martensite start temperature, stabilizes retained austenite (RA), and improves strength and toughness. However, the influence of Ni content on RA characteristics and cryogenic deformation behavior has not been systematically clarified.
This study investigates Fe–xNi–0.3C steels containing 9, 12, 15, and 18 wt.% Ni after quenching, lamellarizing, and tempering (QLT). RA fractions before and after tensile deformation at 77 K were quantified by X-ray diffraction, while electron backscatter diffraction characterized film-like and blocky RA. Cryogenic tensile tests and work-hardening analyses evaluated strength, elongation, and transformation-assisted deformation. Increasing Ni content increased the initial RA fraction and altered its morphology, producing distinct strength–ductility responses. The 18Ni steel exhibited the highest strength, whereas the 15Ni steel achieved the best strength–ductility balance. Cryogenic tensile performance was governed by the combined effects of RA fraction, morphology, and deformation stability. |