| Abstract Scope |
End-of-Life (EOL) NdFeB permanent magnets (PMs) contain 20–30% rare earth elements (REEs), including Nd, Pr, Dy, and Tb. Since REE concentrations are higher than in commercial ores, the EOL magnets can be considered a viable alternative source for securing supply chains. Conventional pyrometallurgical and hydrometallurgical recovery routes require oxidative roasting (>800 °C) to decompose Nd2Fe14B into NdFeO3, NdBO3, and Fe2O3. Subsequent high-temperature carbothermal reduction (1400 °C) of oxidative-roasted NdFeB reduces NdFeO3 to Nd2O3 and Fe. The present study emphasises low-temperature alkali treatment (30% w/w aq. NaOH, 80 °C, 3 h) that decomposes Nd2Fe14B into Nd(OH)3, Fe, and Fe3O4 while leaching boron. This partial oxidation prevents the formation of NdFeO3. Following carbothermal (1400 °C) and hydrogen (100% H2, 800 °C), Fe3O4 is reduced, yielding Nd2O3(s), molten Fe, and Nd2O3(s), Fe (s) phases respectively. Subsequent H2 reduction and inert carbon-saturating smelting of Fe at 1400 °C facilitate solid-liquid separation. |