| Abstract Scope |
The growing demand for LIBs in electric mobility applications contributes to the massive availability of discarded NMC-type batteries. Hydrogen reduction of retrieved cathode powder is employed to selectively recover Li and the values of Ni, Co, and Mn. A systematic investigation combining detailed characterization was conducted to analyze the underlying reduction mechanism. Thermodynamic evaluation and systematic reduction experiments show the dissociation of the stable layered NMC structure to respective metal/oxides above 400 °C followed by water leaching, magnetic separation, and 2 M H2SO4 leaching. 91% Li recovery and 96% Ni, 90% Co, and 94% Mn dissolution at 2 M H2SO4, 60 °C, 60 min, and 50 g/l. The proposed hydrogen reduction of NMC cathode active material is found promising and sustainable for metal recovery.
Keywords: Recycling; Hydrogen; Reduction; Lithium; Cobalt |