| Abstract Scope |
Massive steel slag discharge, iron loss and low tailing utilization remain prominent industrial bottlenecks. Taking converter steel slag as feedstock, this work explores how grinding fineness, magnetic intensity and separation duration affect iron concentrate grade and total iron recovery. Magnetic separation tailings are mechanically activated and compound-modified with gypsum to evaluate their cementitious activity and roadbed filler performance.
Optimal parameters: 85% passing −0.074 mm, 180 mT magnetic field and 8 min separation, yielding concentrate with 68.32% TFe and 59.76% iron recovery. After 45 min mechanical activation plus 3% gypsum modification, tailings achieve 79.2% 7 d and 86.5% 28 d cementitious activity with sound volume stability. This integrated route supports full resource valorization of steel slag. |