About this Abstract |
| Meeting |
2027 TMS Annual Meeting & Exhibition
|
| Symposium
|
Composite Materials for Nuclear Applications IV
|
| Presentation Title |
Investigation of Corrosion Behavior in C-SiC and Cf/C–SiC Ceramic Matrix Composites in Ternary MgCl2-KCl-NaCl Molten Salt |
| Author(s) |
Jagadeesh Sure, Ryan Gordon, Youyang Zhao, Bhagwat Ghule, Kumar Sridharan, Junhua Wei, Adrien Couet |
| On-Site Speaker (Planned) |
Jagadeesh Sure |
| Abstract Scope |
SiC is promising material for nuclear and solar power applications but is brittle and fracture-prone. C or SiC Fiber-reinforced ceramic matrix composites (CMCs) offer superior toughness and damage tolerance. This study evaluates the microstructure and high-temperature corrosion behavior of two CMCs: amorphous carbon matrix-filled SiC nanoparticles (C–SiC) without densification and carbon fiber-reinforced carbon matrix with SiC nanoparticles (Cf/C–SiC) densified by two polymer infiltration and pyrolysis (PIP) cycles using a SiC preceramic resin. Isothermal corrosion tests were performed in MgCl2–KCl–NaCl molten salt at 780 °C for 650 h. C–SiC exhibited significantly higher mass loss (14.4 mg/cm²) than Cf/C–SiC (0.07 mg/cm²). Microscopy revealed severe layer detachment in C–SiC, whereas Cf/C–SiC retained structural integrity. Salt penetration exceeded 40 µm in C–SiC but remained ≤20 µm in Cf/C–SiC. Compared with monolithic CVD SiC, the baseline material, the CMC exhibited 10 times lower mass loss |
| Proceedings Inclusion? |
Planned: |
| Keywords |
Composites, High-Temperature Materials, Nuclear Materials |