About this Abstract |
| Meeting |
2027 TMS Annual Meeting & Exhibition
|
| Symposium
|
Steels in Extreme Conditions III
|
| Presentation Title |
Comparing Stress Corrosion Cracking Behavior of Laser Powder Bed Fusion and Direct Energy Deposition Print Strategies for Additively Manufactured 17-4PH Stainless Steel |
| Author(s) |
Cody Urso, James Burns |
| On-Site Speaker (Planned) |
Cody Urso |
| Abstract Scope |
Stress-corrosion cracking (SCC) behavior of direct energy deposition (DED) 17-4PH stainless steel was characterized and compared with wrought and laser powder bed fusion (LPBF) material. Post-build homogenization, solution annealing, and aging produced a microstructure and peak-aged strength (~1200 MPa) comparable to wrought 17-4PH. SCC susceptibility was evaluated using linear elastic fracture mechanics under both rising- and constant-stress-intensity (K = 30–40 MPa√m) conditions across potentials ranging from mildly anodic to strongly cathodic. Rising-K tests showed similar Stage I behavior for DED and LPBF, while DED exhibited slightly lower Stage II crack growth rates at K = 15–25 MPa√m. Under fixed cathodic conditions, DED displayed a slightly narrower immunity regime than wrought and LPBF. SEM fractography showed similar fracture morphology. EDS and EBSD analyses revealed greater retained austenite and lower porosity in DED than in LPBF, suggesting that these microstructural differences contribute to the observed SCC behavior. |
| Proceedings Inclusion? |
Planned: |
| Keywords |
Environmental Effects, Characterization, Iron and Steel |